Photo Martin Skoliber
Sample 19 is clay from Loka-Črnomelj (White Carniola). The recommended firing temperature is 900–1000 °C. The beginning of sintering is at 1000–1250 °C. At 1000 °C shrinkage is 19 % and porosity 5 %.
Clay samples
800 °C
900 °C
1000 °C
1100 °C
1200 °C
1300 °C
- segrevanje
heating up - priporočena temp. žganja
recommended firing temperatures - začetek sintranja
the beginning of sintering - mehčanje
softening
Clay preparation for testing
unprocessed clay
sifted and dried clay- grain size in mm
0.8 % = 1.0 mm
0.4 % = 0.2 mm
0.2 % = 0.05 mm