sample69Log Čezsoški · Slovene Littoral

46.304120 13.489264

Collected by Jeron Magušar

Urban Magušar in a Clay Warehouse – Log Čezsoški · Slovene Littoral
Urban Magušar in a Clay Warehouse
Photo Jošt Gantar

Sample 69 is clay from Log Čezsoški (Slovene Littoral). The recommended firing temperature is 900–1300 °C. At 1300 °C shrinkage is 0 % and porosity 4 %.

Clay samples

  1. Sample 69 – 800 °C800 °C
  2. Sample 69 – 900 °C900 °C
  3. Sample 69 – 1000 °C1000 °C
  4. Sample 69 – 1100 °C1100 °C
  5. Sample 69 – 1200 °C1200 °C
  6. Sample 69 – 1300 °C1300 °C
segrevanjeheating uppriporočena temp. žganjarecommended firing temperaturesžganje/firing °C%%002244668810101212141416161818202022222424suha glina/dry clay900 °C1000 °C1100 °C1200 °C1300 °C
  • segrevanje
    heating up
%04812162024suhadry9001000110012001300°C
poroznost/porosity %skrčki/shrinkage %

Clay preparation for testing

  1. unprocessed clayunprocessed clay
  2. sifted and dried claysifted and dried clay
  3. 012341.00.20.05%grain size in mm
  4. 1.6 % = 1.0 mm1.6 % = 1.0 mm
  5. 0.3 % = 0.2 mm0.3 % = 0.2 mm
  6. 0.3 % = 0.05 mm0.3 % = 0.05 mm